KIMYA ABS-R Filament – 750 grams
Kimya ABS-R 3D filament is a standard ABS based on 100% post-consumer recycled material from a recycling company based
in France. Its use contributes to the development of a circular economy by reducing the emission of C02, the
consumption of water and electricity as well as the oil resources necessary for its production. Acrylonitrile
butadiene styrene (ABS) is a thermoplastic polymer combining lightness, high impact resistance and good temperature
resistance. ABS is suitable for functional prototyping, enclosure applications in industries such as appliances,
telephony, automotive, hardware and toys.
- Better heat resistance than PLA (around 90°C)
- Good impact resistance
- Made from 100% post-consumer recycled ABS – reduced environmental impact
- Compliant with REACH regulation and RoHS directive
2-year KIMYA warranty.
Store away from light, humidity and heat to maintain the properties of the product.
FILAMENT PROPERTIES
PROPERTIES | TEST METHODS | VALUES |
---|---|---|
Diameter | INS-6712 | 1.75 ± 0.1 mm 2.85 ± 0.1 mm |
Density | ISO 1183-1 | 1.049 g/cm3 |
Moisture rate | INS-6711 | < 0.5% |
Melt flow index (MFI) | ISO 1133-1 (@210°C – 2,16 kg) | 14.2 g/10min |
Glass transition temperature (Tg) | ISO 11357-1 DSC (10°C/min – 20-220°C) | 110 °C |
PRINT PARAMETERS AND SPECIMENS DIMENSIONS
PRINTING DIRECTION | XY |
---|---|
Printing Speed | 20-50 mm/s |
Infill | 100% – rectilinear |
Infill Angle | 45°/-45° |
Nozzle Temperature | 190-210°C |
Bed T° | 20-60°C |
PRINTED SPECIMENS PROPERTIES
PROPERTIES | TEST METHODS | VALUES | |
---|---|---|---|
MECHANICAL PROPERTIES |
Tensile modulus | ISO 527-2/5A/50 | 1,722 MPa |
Tensile Strength | ISO 527-2/5A/50 | 32.2 MPa | |
Tensile strain at strength | ISO 527-2/5A/50 | 2.1 % | |
Tensile Stress at Break | ISO 527-2/5A/50 | 27.5 MPa | |
Tensile strain at break (type A) | ISO 527-2/5A/50 | 9.4 % | |
Flexural modulus | ISO 178 | 1,557 MPa | |
Flexural stress at conventional deflection (3,5% strain)* | ISO 178 | 48.4 MPa | |
Charpy impact resistance | ISO 179-1/1eA | 8.5 kJ/m² | |
Shore Hardness | ISO 868 | 72.2D |
Note 1 |
*According to ISO 178, end of the test at 5% deformation even if there is no specimen break. |
Note 2 |
The data should be considered as indicative values – Properties can be influenced by production conditions. |
PRINT SETTINGS:
- PRINT SPEED: 20-60 mm/s
- EXTRUSION TEMPERATURE: 250-270°C
- PLATFORM TEMPERATURE : 90-110°C
- CHAMBER TEMPERATURE : 20-80°C
MISCELLANEOUS
Spool Material | PC |
Steaming Temperature | 80°C |
Steaming Duration | 2h-4h |
CERTIFICATION AND USES
PROPERTIES | RATING |
Ease to print |
|
Rigidity |
|
Elasticity |
|
Impact Strength |
|
Temperature Resistance |
|
Weather Resistance |
|
RoHs | Compliant |
EU 10/2011 | Non Compliant |
FDA | Non Compliant |
UL94 – V0 | Non Compliant |
ESD Protection | Non Compliant |